Resin Type: Hexene Copolymer, High Antiblock, High Slip, Processing Aid Version of 7105T, Cast/Blown Film Resin Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPE. Slip 2000 ppm. Antiblock 7500 ppm. Applications:Industrial Liners, Carrier Bags, Coextrusions Processing Conditions: Extruder 6.35 cm. Screw L/D Ratio 24:1. Die Opening 0.1905 cm. Blow-Up Ratio 2:1. Film properties below based on film thickness of 31.8 µm. Data provided by Chevron Chemical. |