MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Applied Silicone 40064 RTV Adhesive, Acetoxy Cure, Implant Grade
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Silicone to Silicone Bonding

Information provided by Applied Silicone Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/cc
Solids Content 100 %100 %
Viscosity 150000 cP150000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2424Typical
 20 - 3220 - 32
Tensile Strength >= 3.10 MPa>= 450 psi
 5.38 MPa780 psiTypical
Elongation at Break >= 350 %>= 350 %
 650 %650 %Typical
200% Modulus 0.621 MPa
@Strain 200 %
90.0 psi
@Strain 200 %
Tear Strength >= 7.01 kN/m>= 40.0 pli
 12.3 kN/m70.0 pliTypical
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
 
Descriptive Properties
Cure SystemAcetoxy

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain CHR® M52 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Parker Chomerics Tecknit® 0236 Conductive Silicone Sealant/Adhesive
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
NuSil R-2180 Silicone Engineering Coating
NuSil CF1-6755 Silicone Two Part Sealing & Adhesive

PNUSILA931 / 194600

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.