Forms: Pellets
Filler/Reinforcement: Glass Fiber Reinforcement, 43% Filler by Weight
Additive: Lubricant and Heat Stabilizer
Features: Lubricated, Heat Stabilized and Low Extractables
Appearance: Black
TPCI# 9571102