ELASTOSIL® R plus 533/60 A/B is a two component addition curing HCR silicone for the manufacture of silicone-insulated wires and cables. Properties: The hardness of ELASTOSIL® R plus 533/60 A/B is approximately 68 - 70 Shore A. Special features: - good mechanical and electrical properties
- good rheological properties
- good heat resistance
- in case of fire low smoke density
- low toxicity of the combustion products
- the insulation is free of halogens regardless of the chosen curing method
- the insulation is free from peroxide split products
Application: Heavy duty cables, where low volatiles, good abrasion resistance, high flexing durability or high mechanical strength are required.Information provided by Wacker Chemie AG. |