MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive cooling fans & shrouds, automotive door handles, brackets, automotive mirror shells, painted parts, components for small gas engines, sporting goods, auto luggage rack components.

Data provided by the manufacturer, Wellman Inc.

Key Words: Polyamide 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.46 g/ccISO 1183
Water Absorption 0.80 %Approximate 24 hr.
Linear Mold Shrinkage 0.0020 - 0.0060 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 120 MPaISO 527
Elongation at Break 3.0 %ISO 527
Flexural Yield Strength 185 MPaISO 178
Flexural Modulus 7.50 GPaISO 178
Izod Impact, Notched 0.500 J/cmISO 180
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 200 °CISO 75
Flammability, UL94 HB
@Thickness 1.57 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 530 - 560 °F
Middle Barrel Temperature 520 - 540 °F
Front Barrel Temperature 510 - 530 °F
Nozzle Temperature 490 - 540 °F
Melt Temperature 520 - 570 °F
Mold Temperature 160 - 200 °F
Drying Temperature 175 °FOpened bags and gaylord boxes
Dry Time 2 - 4 hourOpened bags and gaylord boxes
Moisture Content 0.050 - 0.20 %During molding to prevent hydrolytic degradation
 <= 0.20 %In shipping bags, ready to mold
Injection Pressure 5000 - 20000 psi
Back Pressure 50.0 psi
Screw Speed 30 - 120 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Chemlon® 125-15 MGH Nylon 66, 25% Mineral Reinforced, 15% Glass Fiber Reinforced
Teknor Apex Chemlon 225-15 MG Nylon 6, 25% Mineral/15% Glass Fiber Reinforced
Teknor Apex Chemlon 125-15 MG Nylon 66, 25% Mineral/15% Glass Fiber Reinforced
RTP Company RTP PA66 15 GF 25 M BLK Nylon 6/6 (PA), Value Product - 15% Glass Fiber - 25% Mineral - Heat Stabilized
Envalior Akulon® K224-HGM35 (Dry) 15% Glass Reinforced, 25% Mineral Reinforced, Heat Stabilized Nylon 6 (North America)

PWEL48 / 72328

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.