MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chevron Phillips Marlex® 1019 Extrusion Coating Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: This low density polyethylene is tailored for extrusion coating applications that require:
  • Excellent processability
  • Very high line speed at low coating weights
  • Processability at lower extrusion temperature
  • High temperature extrusion stability
  • Excellent drawdown characteristics
  • Low neck-in
Typical extrusion coating applications may include:
  • Food packaging
  • Laminations
  • Sealant resin
  • General paper and board coating
  • General flexible packaging

Data provided by Chevron Chemical.

Formerly branded with the MarFlex® trade name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D1505
Water Vapor Transmission 25.0 g/m²/day1.61 g/100 in²/dayASTM F1249
Oxygen Transmission Rate 7200 cc/m²/day464 cc/100 in²/dayASTM D3985
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 190 °C
16 g/10 min
@Load 4.66 lb,
Temperature 374 °F
ASTM D1238
 
Thermal PropertiesMetricEnglishComments
Melting Point 103 °C217 °FASTM D3418
Vicat Softening Point 87.0 °C189 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Extruded
Kraton® D1102 + LDPE blend (2/98)
Ineos T50-3600 HDPE
EMS-Grivory Grilamid® L 16 nat PA12
Dow FLEXOMER™ ETS-9064 NT 7, 0.8 mil Very Low Density Polyethylene (VLDPE) Resin

PCHEVVD2 / 20533

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.