MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolon® 2612 Polyvinyl Chloride - Polyvinyl Acetate Copolymer
Categories: Polymer; Thermoplastic; Vinyl (PVC); Polyvinyl Chloride - Polyvinyl Acetate Copolymer

Material Notes: F-2612 is a fine particle size vinyl chloride-vinyl acetate copolymer blending resin. It combines the viscosity-reducing properties with the lower gelling temperatures of vinyl acetate copolymer. It has been designed for using in applications where rapid gelatin and fusion is a requirement, due to low processing temperatures.

Information provided by Formosa Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.550 g/ccQC-10-105
Volatiles 0.30 %ASTM D 3030
Particle Size 32 µmAverage; Coulter Counter LS230
Relative Viscosity 1.95 cPASTM D2857
Vinyl Acetate Content 12 %QC-10-105
 
Descriptive Properties
Inherent Viscosity0.77ASTM D1243
K-Value59Fikentscher’s Constant
Sieve Analysis100 percentASTM 1921(B). Through 40 Mesh Screen
 99 percentASTM 1921(B). Through 200 Mesh Screen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyvinyl Chloride - Polyvinyl Acetate Copolymer
Inovyn 557RA Copolymer of Vinyl Chloride and Vinyl Acetate
SEKISUI SPI KYDEX® 5555 Acrylic/PVC
Inovyn 550GA Copolymer of Vinyl Chloride and Vinyl Acetate
Inovyn 561SF Vinyl Chloride - Vinyl Acetate copolymer Paste - filler

PFPCPQ9001 / 239822

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.