MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

American Elements Iron Nickel Nanopowder
Categories: Metal; Ferrous Metal

Material Notes: General Description

Iron Nickel ( FeNi) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area nanocrystalline alloy particles with magnetic properties. Nanoscale Iron Nickel Particles are typically 20-40 nanometers (nm) with specific surface area (SSA) in the 30 - 50 m 2 /g range and also available in with an average particle size of 100 nm range with a specific surface area of approximately 7 m 2 /g. Nano Nickel Iron Particles are also available in ultra high purity and high purity and coated and dispersed forms. Applications for Iron Nickel Nanocrystals include as an hydrogenation catalyst and as a reagent for the dehalogenation of trichloroethylene (TCE), a common groundwater environmental remediation contaminant, in electro magnetic machines and in coatings, plastics, nanowire, and in certain alloy and catalyst applications. Further research is being done for their potential electrical, dielectric, magnetic, imaging, catalytic, bio-medical and bioscience properties.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 0.030 - 0.050 µm0.030 - 0.050 µm
 0.10 µm0.10 µm
Specific Surface Area 7.0 m²/g7.0 m²/g
 30 - 50 m²/g30 - 50 m²/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for AISI 4000 Series Steel
Mid-Mountain Materials ARMATEX® SF17 Industrial Silicone Rubber Coated Glass Fabric
American Elements Iron Cobalt Nanopowder
Overview of materials for Austenitic
Overview of materials for Chrome-moly Steel

EJAMER43 / 5526

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.