Greenflex ML 60 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 60 show very high elasticity. Main Applications: Greenflex ML 60 is recommended for the production of foamed and crosslinked sheets for shoes and gaskets. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |