MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Silfoam® SC 1132 Silicone Antifoam Compound
Categories: Fluid

Material Notes: SILFOAM® SC 1132 is an opaque, viscous, anhydrous compound that is effective against a wide range of surfactants.

Application: SILFOAM® SC 1132 is based on high-molecular polysiloxanes and has a mean viscosity of 30.000 mPa*s at 25°C. Even in small amounts it is highly effective in suppressing foam in detergents and systems with high surfactant content. SILFOAM® SC 1132 can be used for the production of antifoam powders for post-addition to powder detergents as foam suppressor. SILFOAM® SC 1132 is an excellent defoamer for structured liquid detergents and it is a good deaerating agent and defoaming agent for gel products. SILFOAM® SC 1132 can be also used for slurry deaeration.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 - 1.04 g/cc0.0358 - 0.0376 lb/in³DIN 12791
Volatiles 0.00 - 1.5 %
@Temperature 150 °C,
Time 7200 sec
0.00 - 1.5 %
@Temperature 302 °F,
Time 2.00 hour
5g
Brookfield Viscosity 30000 cP30000 cPdynamic, spindle 3/ 2.5 rpm
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.40 - 1.411.40 - 1.41DIN 51423
 
Descriptive Properties
Active ingredients (%)100
Appearanceslightly opaque, colorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Silfoam® SC 385 Silicone Antifoam Compound
Wacker Pulpsil® 355 Silicone Antifoam Compound
Dow Y-30 ANTIFOAM EMULSION
Dow 2210 ANTIFOAM

PWACK9444 / 204973

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.