MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
Saint-Gobain Meldin® 5320 Thermoplastic Bearing Material
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: General Notes on Meldin 3000/5000 Series Bearing Products:
Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.
Specific Notes on Meldin® 5230 Bearing
Meldin 5320 components supply substantial strength and rigidity. They maintain high tensile, flexural, and compressive properties, even at elevated temperatures.

Applications include:Compressor Valve Plates and Valve Rings, Transmission Thrust Washers and Rings, and Vanes for Air Motors and Pumps
Information provided by Saint Gobain Performance Products.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D792
Water Absorption 0.11 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 103ASTM D785
Tensile Strength 156 MPaASTM D638
Elongation at Break 2.1 %ASTM D638
Elongation at Yield 2.7 %ASTM D638
Flexural Strength 250 MPaASTM D790
Flexural Modulus 9.60 GPaASTM D790
Compressive Strength 214 MPaASTM D695
Izod Impact, Notched 120 J/m
Izod Impact, Unnotched 720 J/m
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.2
@Frequency 1000 Hz
ASTM D149
Dielectric Strength 510 V/mil
@Thickness 2.50 mm
ASTM 149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µm/m-°C
@Temperature 23.0 - 143 °C
Below Tg; ASTM E831
 110 µm/m-°C
@Temperature >=143 °C
Above Tg; ASTM E831
CTE, linear, Parallel to Flow 18.0 µm/m-°C
@Temperature 23.0 - 143 °C
Below Tg; ASTM E831
 18.0 µm/m-°C
@Temperature >=143 °C
Above Tg; ASTM E831
Thermal Conductivity 0.420 W/m-KASTM F433
Melting Point 343 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 316 °CASTM D648
Glass Transition Temp, Tg 143 °CASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® SCP-5009 Polyimide
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material
Saint-Gobain Meldin® 5025 Bearing
Saint-Gobain Meldin® 5330 Thermoplastic Bearing Material

PSTGQ995 / 108540

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.