Resin Type: homopolymer Characteristics: excellent flexibility, excellent flow, good warping resistance, moderate mold release, moderate ESCR Applications: large housewares, tamper evident snap-on caps, feminine hygiene applications Information provided by Chevron Phillips Chemical Company. |