Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospace applications. Key Features and Benefits: - Excellent retention of mechanical properties after long-term high temperature exposure
- Soft tack and drape properties
- Long ambient out-time for maximum process flexibility
- Good electrical properties for RF applications
- Meets requirements of MIL-R-9300B Type II
Applications/Qualifications: - Secondary Aircraft Structures
- Radomes
- Nacelles
- Inlet Ducts
- Fairings
- Meets SS9578 and GMS4001 specifications.
Information provided by Park Electrochemical Corp. |