MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Gougeon Brothers PRO-SET® HTP 187/HTP 288 High-Temp Surface Coat Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: High-temperature, high-performance epoxy surface coat formulation for synthetic composite parts and tooling manufacturing. Black in color.
Tg as high as 270°F (132°C) with proper post-cure. Provides excellent temperature stability and great part cosmetics.
Slow cure speed provides 2 to 3 hours working time at 72°F (22°C). A second application can be applied while the first coat is tacky, which is typically after 6-8 hours. After 24 hours cure at 72°F (22°C) the laminating process can begin.
Medium Viscosity enables brush application and air release. Easily applied with a short bristle brush.
Thixotroped to prevent runs and sags at a thickness of 10-12 mils.
Elevated temperature cure is required. The surface coat and laminate should be post cured together. See chart for post cure information.

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccHardener
 1.21 g/ccCured
 1.29 g/ccResin
Viscosity 900 cP
@Temperature 22.0 °C
hardener; ASTM D2196
 4900 cP
@Temperature 48.9 °C
Mixed
 7700 cP
@Temperature 29.4 °C
Mixed
 17500 cP
@Temperature 22.8 °C
Mixed
 18000 cP
@Temperature 29.0 °C
Mixed; ASTM D2196
 24000 cP
@Temperature 22.0 °C
resin; ASTM D2196
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 92RT + 60°C x 2hr + 135°C x 12hr; ASTM D2240
Tensile Strength 3700 psiRT + 60°C x 2hr + 135°C x 12hr; ASTM D638
Elongation at Break 0.90 %RT + 60°C x 2hr + 135°C x 12hr; ASTM D638
Tensile Modulus 560000 psiRT + 60°C x 2hr + 135°C x 12hr; ASTM D638
Flexural Strength 7900 psiRT + 60°C x 2hr + 135°C x 12hr; ASTM D790
Flexural Modulus 410000 psiRT + 60°C x 2hr + 135°C x 12hr; ASTM D790
Compressive Yield Strength 21000 psiRT + 60°C x 2hr + 135°C x 12hr; ASTM D695
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 247 °FRT + 60°C x 2hr + 135°C x 12hr; ASTM D648
Glass Transition Temp, Tg 268 °FRT + 60°C x 2hr + 135°C x 12hr, DMA Onset Storage Modulus, 1 Hz, 3°C per minute; ASTM E1640
 291 °FRT + 60°C x 2hr + 135°C x 12hr, DSC Onset– 1st Heat; ASTM E1356
 297 °FRT + 60°C x 2hr + 135°C x 12hr, DMA Peak Tan Delta, 1 Hz, 3°C per minute; ASTM E1640
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourtypical laminate will be gelled
Pot Life 150 min
@Load 0.500 kg
ASTM D2471
 160 min
@Load 0.150 kg
ASTM D2471
Working Life 2.00 - 3.00 hour
Shelf Life 18.0 Monthhardener
 36.0 Monthresin
 
Descriptive Properties
Mix ratio100:10.5 - 100:13.3Weight Range, Resin: Hardener
 100:11.7Weight, Resin: Hardener
 100:12.8 - 100:16.3Volume Range, Resin: Hardener
 100:14.3Volume, Resin: Hardener
 7.00:1Volume, Resin: Hardener
 7.79:1 - 6.15:1Volume Range, Resin: Hardener
 8.53:1Weight, Resin: Hardener
 9.50:1 - 7.50:1Weight Range, Resin: Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOUGP947 / 290790

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.