MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nouryon Accelerator CF32 Metal complex
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Accelerator CF32 is a cobalt-free accelerator for curing thermoset resins.

Applications: Accelerator CF32 can be used in combination with Butanox M-50 and most other peroxides, such as Butanox LPT and Trigonox K-90 in ambient and in some cases also at elevated temperature curing for most commonly used UP and VE resins. The material is suitable for most thermoset applications, including ambient temperature curing in: hand lay-up and spray-up application, polymer concrete manufacturing, discontinuous filament winding (pipes and storage tanks manufacturing). In combination with Trigonox K-90 curing at elevated temperature is possible in applications such as: continuous filament winding (pipes manufacturing). Furthermore, Accelerator CF32 might be considered in other applications and market segments where Cobalt is an undesired component.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
AppearanceClear green liquid
Content285-345 mg/kgIron

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY010 / 285533

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.