MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT KÖRAFORM K 20 Silicone Elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: This is a two-component room temperature condensation curing silicone compound. The cured product is an exceptionally flexible rubber with very high mechanical properties and good shelf life stability. It is suitable for mould making of intricate patterns with extremely good pick up of fine details. Softer grades are better suited for use where there are deep undercuts

Key Features

  • High stability, ideal for building up the wall thickness on vertical surfaces
  • Very good elastic properties
  • Skin moulds with strong undercuts
  • Moulds for stucco plasterers
Application: Moulds for stucco plasterers

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccB; BS ISO 2781
 1.10 g/ccCured Product; BS ISO 2781
 1.13 g/ccA; BS ISO 2781
Brookfield Viscosity 20 cPB
Linear Mold Shrinkage 0.0060 cm/cm
Storage Temperature 5.00 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40DIN 53 505
Tensile Strength 290 psiDIN 53 504, S 3 A
Elongation at Break >= 500 %DIN 53 504, S 3 A
Tear Strength 92.0 pliASTM D 624, Die B
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hourDe-mould Time / Full Cure
Pot Life 30.0 min
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceBlue
ColorColorless / blueB
 OpaqueA
 Opaque/colorless to blueCured Product
Cure typeCondensation
Mix Ratio100:5By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL140 / 314623

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.