MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kolon CS301 Heat shrinkable PET Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Ant-stat treatment. Polyester film designed for packaging, bottle label, cap sealing, etc. It can be treated with coating materials in order to offer slippery, good wetting on paint and adhesive and anti-static properties.

Information provided by Kolon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 30.0 - 70.0 microns1.18 - 2.76 mil
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD >= 400 %>= 400 %
Film Elongation at Break, TD 50 %50 %
Coefficient of Friction, Dynamic <= 0.50<= 0.50
Coefficient of Friction, Static <= 0.50<= 0.50
Film Tensile Strength at Break, MD >= 49.0 MPa>= 7110 psi
Film Tensile Strength at Break, TD >= 196 MPa>= 28400 psi
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1.00e+12 ohm<= 1.00e+12 ohm
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD <= 5.0 %<= 5.0 %Heat Shrinkage
Shrinkage, TD >= 75 %>= 75 %Heat Shrinkage

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Armacell ArmaForm® PET Foil 70
DuPont Teijin Films Melinex® HC-1 Planarised PET film
Eastman 9921 PET Film
Solvay P720X PET-Based Release Film
Armacell ArmaFORM® PET Foil 70

PKOKZ825 / 185368

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.