MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil 75W-80 Mobilfluid LT
Categories: Fluid; Lubricant

Material Notes: Mobilfluid LT is an extra high performance multipurpose tractor lubricant engineered to meet or exceed tractor transmission, drivetrain, and hydraulic fluid requirements. This product is designed to optimize the performance of agricultural and industrial tractors operating in a wide range of environments and especially in low ambient temperature applications. This next generation product combines select base oils and an advanced additive package to deliver a variety of lubricant performance properties required by various applications.

Heavy-duty transmissions, differentials, final drives, hydraulic systems, power steering systems, wet brakes, PTOs, and hydrostatic drives used in agricultural, contractor, and industrial applications; Recommended for top-up and refill of systems; Suitable for transmission applications requiring Type A (Suffix A), Dexron, and Type F fluids; Recommended for hydraulic and transmission systems where an SAE 10W-20 engine oil is specified; Do not use in passenger car automatic transmissions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.875 g/cc
@Temperature 15.0 °C
0.0316 lb/in³
@Temperature 59.0 °F
ASTM D4052
Brookfield Viscosity 20000 cP
@Temperature -40.0 °C
20000 cP
@Temperature -40.0 °F
Viscosity Measurement 180180Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 34 cSt34 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 7.2 cSt7.2 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -45.0 °C-49.0 °FASTM D97
Flash Point 198 °C388 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON062 / 75487

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.