MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Gougeon Brothers West System® Six10 Thickened Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: WEST SYSTEM® Six10 Thickened Epoxy Adhesive is a pre-thickened, gap-filling epoxy with a smooth, non-sagging consistency that trowels easily—perfect for filling voids and making fillets. Six10 has a viscosity high enough to resist sagging but can still saturate and wet-out a surface without pre coating, thanks in part to a property called shear thinning. This property also enables it to wet out light to moderate weight reinforcing fabrics such as fiberglass and carbon fiber. Six10 is packaged in a specially designed, self-metering cartridge. A unique piston inside the cartridge simultaneously dispenses the resin and hardener from separate chambers. The molded chambers and passageways accurately control the ratio and prevent the resin and hardener from contacting each other until they are outside the cartridge and pass through the 600 Static Mixer. The Six10 Epoxy formulation is a good balance between the elongation and toughness of G/flex® and the strength and stiffness of our 105 Resin-based epoxies. It has a long open time which means the epoxy will stay workable for 42 minutes in the static mixer and before clamping is required—very practical for long or complicated assemblies. It is ideal for stitch and glue boat construction, fiberglass laminate repair and general bonding. It bonds to a wide range of materials including wood, metals, composites and masonry. Six10 is transparent with a straw yellow tint.

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80.680.6ASTM D-2240
Tensile Strength 44.4 MPa6440 psiASTM D638
Elongation at Break 7.9 %7.9 %ASTM D638
Tensile Modulus 2.56 GPa371 ksiASTM D-638
Flexural Strength 77.9 MPa11300 psiASTM D-790
Flexural Modulus 2.42 GPa351 ksiASTM D-790
Compressive Yield Strength 66.8 MPa9690 psiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 52.8 °C127 °FASTM D-648
Glass Transition Temp, Tg 52.8 °C127 °FOnset
 56.1 °C133 °FUltimate
 
Processing PropertiesMetricEnglishComments
Cure Time 300 - 360 min5.00 - 6.00 hourInitial cure
 1440 - 5760 min24.0 - 96.0 hourWorkable cure
Pot Life 45.0 min45.0 min100 g
Working Life 42.0 min42.0 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOUGW901 / 290745

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.