MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Glyptal C1968 High Solid Gray Primer/Topcoat
Categories: Fluid

Material Notes: GLYPTAL C-1968 is designed to be used where excellent functional properties are a must. Its excellent resistance to topcoat lifting extends its use into areas where excellent exterior topcoats (2-package urethanes) are needed.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 11.67 lb/gal
Solids Content 50 - 54 %Volume
 70 - 74 %Weight
Volatile Organic Compounds (VOC) Content <= 336 g/l
Thickness 1.50 - 2.50 milDry Film
 
Mechanical PropertiesOriginal ValueComments
Impact Test 120 in-lbDirect Impact Resistance; at one week
 
Thermal PropertiesOriginal ValueComments
Flash Point <= 100 °Fcc/pm
 
Optical PropertiesOriginal ValueComments
Gloss 5.0 - 15 %60°
 
Processing PropertiesOriginal ValueComments
Dry Time 2.00 hourHandle
Cure Time 0.750 hourTackfree
 
Descriptive Properties
Adhesion1Cross Hatch
Chemical Resistance>500Salt Fog
ColorGray
MethodAir or Airless
Viscosity17-21 secZahn #3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Europrene Latice® 2430 Styrene - Butadiene Copolymer
Nanocyl SIZICYL™ XC R2G Liquid Sizing Agent for Carbon and Glass Fibers
Versalis Europrene Latice® 5577 Styrene - Butadiene Copolymer
Versalis Europrene Latice® 5570 Styrene - Butadiene Copolymer
Versalis Intex® 84 Styrene - Butadiene Copolymer

PGLYPT926 / 209765

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.