MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Silfoam® SC 385 Silicone Antifoam Compound
Categories: Fluid

Material Notes: SILFOAM® SC 385 is a medium viscosity antifoam agent that has an active ingredient content of 100 % and is based on an organically modified silicone fluid. In comparison to antifoam agents which are based on pure silicone fluids (PDMS), SILFOAM® SC 385 in general exhibits better compatibility with organic systems.

Application: SILFOAM® SC 385 is ideal for aqueous and solvent borne applications in which silicones would usually cause problems: manufacture and processing of dispersions, paints and surface coatings, adhesives, cooling lubricants, textile applications and degassing of epoxy and polyurethane resins.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.985 g/cc0.0356 lb/in³DIN 57175
Viscosity 300 cP300 cPdynamic
 
Thermal PropertiesMetricEnglishComments
Flash Point 118 °C244 °FISO 2719
Ignition Temperature 380 °C716 °Fliquids; DIN 51794
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4391.439DIN 51423
 
Descriptive Properties
Appearanceyellowish, opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Silfoam® SC 1132 Silicone Antifoam Compound
Wacker Pulpsil® 355 Silicone Antifoam Compound
Dow Y-30 ANTIFOAM EMULSION
Dow 2210 ANTIFOAM

PWACK9443 / 204972

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.