MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

MetalTek MTEK CA20NW Cast UNS J91631 Martensitic Stainless Steel
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; Cast Stainless Steel

Material Notes: Information provided by MetalTek

Key Words: Cast UNS J91631; AMS 5354 (Investment Casting); Wrought UNS S41800; Wrought Grade Greek Ascoloy®
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 302 - 352302 - 352
Tensile Strength, Ultimate >= 1000 MPa>= 145000 psi
Tensile Strength, Yield >= 790 MPa>= 115000 psi
Elongation at Break >= 10 %>= 10 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.15 - 0.20 %0.15 - 0.20 %
Chromium, Cr 12 - 14 %12 - 14 %
Iron, Fe 77.6 - 83.55 %77.6 - 83.55 %As Balance
Manganese, Mn <= 1.0 %<= 1.0 %
Molybdenum, Mo <= 0.50 %<= 0.50 %
Nickel, Ni 1.8 - 2.2 %1.8 - 2.2 %
Silicon, Si <= 1.0 %<= 1.0 %
Tungsten, W 2.5 - 3.5 %2.5 - 3.5 %
 
Descriptive Properties
Heat TreatmentAnneal/Hard & Temper

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cast Stainless Steel CA15B
Cast Stainless Steel CB7Cu-1, ASTM A747
AISI 302 Cast Stainless Steel, ASTM A276 Hot Formed
Cast Stainless Steel CA6N, ASTM A743
AISI 304 Cast Stainless Steel, ASTM A276 Hot Formed

NMETEK069 / 18319

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.