Description: Technipol 232 is an experimental co-polyester based thermoplastic adhesive designed for the production of air and oil filters in the automotive industry. Technipol 232 is an innovative development of Technipol 32 which, maintaining the performances of Technipol 32, achieves the double goal of a raw material cost reduction combined with a significant progress towards the circular economy model.50% of monomers used in the synthesis of Technipol 232 comes either from renewable sources (derivates of not edible vegetable oils) either from the selection and the treatment of post-consumer wastes. It is characterized by good chemical and thermal resistance and a high flexibility, that assures the integrity of the filter during all production steps.Information provided by SIPOL SpA |