Taiwan Sheen Soon Sheenthane® A9550 Thermoplastic Polyurethane Elastomer
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyurethane TPE
;
Polyurethane, TP
;
Thermoplastic Polyurethane, Elastomer, Ether Grade
Material Notes:
Thermoplastic polyurethane elastomer for injection molding
Polyether grade
Information provided by Taiwan Sheen Soon Co., LTD.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.16
g/cc
0.0419
lb/in³
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
93 - 97
93 - 97
Tensile Strength
39.2
MPa
5690
psi
Elongation at Break
450 %
450 %
100% Modulus
12.24
MPa
@Strain 100 %
1775
psi
@Strain 100 %
300% Modulus
22.1
MPa
@Strain 300 %
3200
psi
@Strain 300 %
Processing Properties
Metric
English
Comments
Processing Temperature
190
-
210
°C
374
-
410
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Taiwan PU Corporation TPUI-G95 High Wear Resistance, Injection Molding Polycaprolactone Base TPU
SK Chemicals SKYTHANE® 398A S series Polyurethane
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane
Huntsman IROGRAN® A 98 H 4661 Polyester-Based TPU-Injection Molding Grade
PSHEEN884 / 156288
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.