MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eifeler Coatings Technology ZrN PVD Coating
Categories: Ceramic; Nitride; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Key Characteristics: decorative color, good wear and corrosion resistance

Primary Applications: cast aluminum and generally non-ferrous materials machining; machining of fiberglass, nylon and most polymer materials; forming and punching - reduced cold welding; decorative applications; orthopedic instrumentation

Information provided by Eifeler Coatings Technology

Key Words: Zirconium nitride
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1.00 - 4.00 microns
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 2500 - 3100
Coefficient of Friction 0.50dry, steel
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 600 °C
 
Descriptive Properties
Colorpale yellow

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zirconium Boride, ZrB2
Zirconium Nitride, ZrN
Copper, UNS C12000
H.C. Starck Grade B Zirconium Diboride, ZrB2
High-Conductivity Oxygen-Free Copper hardened 0.015-0.040 mm grain size

NEIFEL003 / 175958

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.