MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chengdu Letain PL003 PPS
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Resin of LTP PL serials is pure PPS resin with high density and molecular weight. Modified reinforced materials and coating materials can be produced base on this kind of resin

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.34 - 1.36 g/cc0.0484 - 0.0491 lb/in³GB1033
Water Absorption 0.50 %0.50 %GB1034
Melt Flow 25 - 700 g/10 min25 - 700 g/10 minGB3682
Ash 0.15 %0.15 %GB9345
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 90.0 MPa13100 psiGB/T1040
Elongation at Break 20 %20 %GB/T1040
Flexural Strength 100 MPa14500 psiGB1042
Izod Impact, Notched (ISO) 12.0 kJ/m²5.71 ft-lb/in²GB/T1043
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmGB/T1410
Surface Resistance 1.00e+16 ohm1.00e+16 ohmGTB/T1410
Dielectric Constant  3.0
@Frequency 1000 Hz
3.0
@Frequency 1000 Hz
GB1409
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
GB1409
Dissipation Factor  0.00060
@Frequency 1000 Hz
0.00060
@Frequency 1000 Hz
GB1409
 0.0015
@Frequency 1e+6 Hz
0.0015
@Frequency 1e+6 Hz
GB1409
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 110 °C230 °FGB1634
 
Descriptive Properties
ColorLight yellow granular

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGLT012 / 255865

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.