MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Alliance C-9 Strontium Ferrite Ceramic Magnetic Material  (discontinued **)
Categories: Ceramic; Oxide

Key Words: Magnet Magnets
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.80 - 5.00 g/cc0.173 - 0.181 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 450 - 580450 - 580
Tensile Strength, Ultimate 20.0 - 50.0 MPa2900 - 7250 psi
Modulus of Elasticity 150 GPa21800 ksi
Flexural Strength 55.0 MPa7980 psi
Compressive Strength 700 MPa102000 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00 ohm-cm>= 1.00 ohm-cm
Magnetic Coercive Force, Hc 3200 Oe3200 Oe
 3300 Oe3300 OeIntrinsic
Magnetic Remanence, Br 4100 Gauss4100 Gauss
Magnetic Maximum Energy Product, BH 4.0 MGOe4.0 MGOe
Curie Temperature 450 °C842 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 9.00 - 9.50 µm/m-°C
@Temperature 20.0 °C
5.00 - 5.28 µin/in-°F
@Temperature 68.0 °F
Parallel DOM
CTE, linear, Transverse to Flow 8.00 µm/m-°C
@Temperature 23.0 °C
4.44 µin/in-°F
@Temperature 73.4 °F
Perpendicular to M
Maximum Service Temperature, Air 350 °C662 °F
 
Descriptive Properties
Reversible Temp Coef., Bd-0.20 %/°C
Reversible Temp Coef., Hd+0.35 %/°C
Temperature Coefficient, Br-0.18 %/°C(20-100°C)
Temperature Coefficient, Hci+0.4 %/°C(20-100°C)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material
Alliance C-7 Strontium Ferrite Ceramic Magnetic Material
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material
Alliance C-8 Strontium Ferrite Ceramic Magnetic Material

NALLIAN38 / 14863

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.