MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Phillips 66 Super-STA® NLGI Grade 1
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Super-STA and Super-STA M are adhesive, multipurpose, extreme-pressure (EP) lithium greases developed for use in a wide variety of automotive and industrial applications. They contain a tackiness additive for improved retention, reduced leakage and enhanced resistance to water washout. Super-STA and Super-STA M are manufactured with high-quality base oils and lithium 12-hydroxystearate soap thickener. They are fortified with extreme-pressure and antiwear additives, rust and oxidation inhibitors, and a tackiness additive. They have good oxidation resistance, high load-carrying capacity for excellent wear protection, and protect metal parts against rust and corrosion. They provide good adhesion to bearing surfaces for improved retention and resistance to water washout, and have excellent resistance to structural breakdown even under severe operating conditions. Super-STA M is the same as Super-STA, but fortified with 1% molybdenum disulfide for extra protection under heavy or shock loading.

Applications:

  • Automotive chassis parts such as steering knuckles, ball joints, U-joints and tie-rod ends
  • Wheel bearings on passenger cars and heavy equipment equipped with drum brakes
  • Moderately loaded plain and rolling-element bearings in industrial equipment
  • Agricultural and construction equipment where a tacky, water-resistant, extreme-pressure lithium grease is required
  • General-purpose shop/industrial grease
Super-STA M No. 2 is recommended for use where the OEM specifies:
  • Mack MG-C for chassis lubrication
Features/Benefits:
  • Multipurpose grease for use in a wide variety of industrial and automotive applications
  • Good extreme-pressure and antiwear properties
  • Good tackiness for improved retention
  • High shear stability
  • Protects against rust and corrosion
  • Resists water washout
  • Protects against fretting in splined shafts, pivot pins and other parts subject to oscillation, sliding or vibration (Super-STA M)

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.856 g/cc0.0309 lb/in³
Viscosity Measurement 9595Index
Saybolt Viscosity at 100°F 1000 SUS1000 SUS
Saybolt Viscosity at 210°F 88 SUS88 SUS
Kinematic Viscosity at 40°C (104°F) 190 cSt190 cSt
Kinematic Viscosity at 100°C (212°F) 17 cSt17 cSt
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)ASTM D2596
Four Ball Wear 0.420 mm0.0165 inScar Diameter; ASTM D4172
Penetration 310 - 340310 - 340
Timken Test 20400 g45.0 lbOK Load; ASTM D2509
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -18.0 °C-0.400 °F
Dropping Point 200 °C392 °F
 
Descriptive Properties
ColorAmber
ThickenerLithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON5143 / 198396

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.