MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

CHT Group QSil 561 Addition Cure Potting Material
Categories: Polymer; Thermoset; Silicone

Material Notes: Product Description: QSil 561 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a flame retardant, thermally conductive, low modulus material that is readily repairable.

Key Features:

  • 100% solids - no solvents
  • Fast curing
  • Low modulus
  • Good elongation

Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.58 g/cc1.58 g/ccUncatalyzed, QSil 561A
 1.58 g/cc1.58 g/ccUncatalyzed, QSil 561B
Viscosity 7500 cP7500 cPUncatalyzed, QSil 561B
 9000 cP9000 cPUncatalyzed, QSil 561A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060Cure 15 minutes at 150°C
Tensile Strength 1.72 MPa250 psiCure 15 minutes at 150°C
Elongation at Break 125 %125 %Cure 15 minutes at 150°C
Tear Strength 3.51 kN/m20.0 pliCure 15 minutes at 150°C
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
Dielectric Constant 3.2
@Frequency 1000 Hz
3.2
@Frequency 1000 Hz
Dissipation Factor 0.00200.0020
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.620 W/m-K4.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 240 °C464 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 150 °C
0.250 hour
@Temperature 302 °F
As Tested
Gel Time 10.0 min10.0 minCatalyzed
 
Descriptive Properties
ColorBeigeUncatalyzed, QSil 561B
 Dark GrayUncatalyzed, QSil 561A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ITW Insulcast® 961 FR Epoxy Potting/Encapsulation Compound
CHT Group QSil 553LV Addition Cure Potting Material
CHT Group QSil 266 Addition Cure Potting Material

PACC2099 / 199487

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.