MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kolon KompoGTe® LN1G30BL Polypropylene with 30% Long Glass Fiber
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: PP LFT +GF 30%

KompoGTe® LFT is produced by impregnation of long fibers into thermoplastics. This provides superior properties compared with short fiber reinforced thermoplastic. Also, it enables production of parts with a higher content of fibers. It is used to replace metal for many industries, such as automotive, electricity & electronics, and other applications. KompoGTe® LFT has homogenized fiber dispersion and excellent impregnation which can lead to superior surface properties and mechanical strength. Processed by injection molding.

Information provided by Kolon Plastic, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 180 MPa
@Thickness 3.20 mm
26100 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Strength 260 MPa
@Thickness 6.40 mm
37700 psi
@Thickness 0.252 in
10 mm/min; ASTM D790
Flexural Modulus 8.85 GPa
@Thickness 6.40 mm
1280 ksi
@Thickness 0.252 in
10 mm/min; ASTM D790
Izod Impact, Notched 1.85 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
3.47 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F20°C/min; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FASTM D648
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 220 - 240 °C428 - 464 °F
Middle Barrel Temperature 240 - 260 °C464 - 500 °F
Front Barrel Temperature 245 - 265 °C473 - 509 °F
Nozzle Temperature 250 - 270 °C482 - 518 °F
Mold Temperature 60.0 - 100 °C140 - 212 °F
Drying Temperature 80.0 - 90.0 °C
@Time 14400 - 21600 sec
176 - 194 °F
@Time 4.00 - 6.00 hour
Dehumidifying Dryer
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOKZ758 / 255769

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.