MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Reynolds TASK® 16 Fast-setting Shore 80A/30D urethane
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: TASK™16 is a low odor, fast-setting Shore 80A/30D urethane that offers very high tear strength, impact resistance and wear resistance. TASK™16 is phthalate free, mercury free and MOCA free. Mixed one part A to two parts B by weight, TASK™16 pours easily. Working time is 6 minutes and handling time is 90 minutes at room temperature. Cured rubber has exceptional performance characteristics and dimensional stability. TASK™ 16 can be colored with SO-Strong™ or Ignite™ colorants. TASK™16 is suitable for making fast mechanical parts, gaskets, wheels and pullies, impact resistant props, and archival master models. It is also used to make fast, wear resistant rubber molds for casting concrete or concrete stamping pads. TASK™16 is also an excellent choice for rotocasting to create hollow semi-rigid castings.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D-1475
Viscosity 1400 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.0025 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D-2240
Hardness, Shore D 30ASTM D-2240
Tensile Strength, Ultimate 2264 psiASTM D-412
Elongation at Break 233 %ASTM D-412
100% Modulus 855 psiASTM D-412
Tear Strength 197 pliDie C; ASTM D-624
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.59
@Frequency 1e+6 Hz
ASTM D150-87
Dissipation Factor 0.064
@Frequency 1e+6 Hz
ASTM D150-87
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
 90.0 minHandling Time
Pot Life 6.00 minASTM D-2471
 
Descriptive Properties
ColorLight Yellow
Mix Ratio1A:2Bby weight
Specific Volume25.6[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN042 / 296743

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.