MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Global J-1600 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Description-suitable for injection molding
Applications-household products, handy craft flowers, toys, stationary

Information provided by Global Polymers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.958 g/cc0.0346 lb/in³ASTM D1505
Environmental Stress Crack Resistance 2.0 hour2.0 hourASTM D1693
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
12 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ASTM D2240
Tensile Strength, Ultimate 19.6 MPa2840 psiASTM D638
Tensile Strength, Yield 28.4 MPa4120 psiASTM D638
Elongation at Break 500 %500 %ASTM D638
Flexural Modulus 0.981 GPa142 ksiOlsen Stiffness; ASTM D747
Izod Impact, Notched 0.196 J/cm0.367 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 131 °C268 °FASTM D2117
Vicat Softening Point 122 °C252 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ethydco Advancene™ EM-6308-UV High Density Polyethylene Resin
Global 110 Polypropylene
Ineos T50-500-196 Polyethylene Copolymer
LyondellBasell Alathon® M5562 High Density Polyethylene
LyondellBasell Alathon® M6580 High Density Polyethylene

PGLOBE04 / 42053

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.