MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI adhesives

(Viewing data as-entered. Click here to return)
Multibase C6-350 LH Parts A and B Dow-Corning Class VI Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Information provided by Multibase

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccRelative; ASTM D792V
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 49no post cure; ASTM D2240
 56post cured- 2 hours at 177°C; ASTM D2240
 56post cured- 4 hours at 177°C; ASTM D2240
 57post cured- 8 hours at 177°C; ASTM D2240
Tensile Strength, Ultimate 1130 psipost cured- 8 hours at 177°C; ASTM D412
 1155 psipost cured- 2 hours at 177°C; ASTM D412
 1172 psipost cured- 4 hours at 177°C; ASTM D412
 1238 psino post cure; ASTM D412
Tensile Strength, Yield 321 psiat 200%, no post cure; ASTM D412
 491 psi200%, post cured- 4 hours at 177°C; ASTM D412
 506 psiat 200%, post cured- 2 hours at 177°C; ASTM D412
 524 psi200%, post cured- 8 hours at 177°C; ASTM D412
Elongation at Break 473 %post cured- 8 hours at 177°C; ASTM D412
 510 %post cured- 4 hours at 177°C; ASTM D412
 511 %post cured- 2 hours at 177°C; ASTM D412
 732 %no post cure; ASTM D412
Tear Strength 216 pliDie B, no post cure; ASTM D624
 242 pliDie B, post cured- 8 hours at 177°C; ASTM D624
 247 pliDie B, post cured- 2 hours at 177°C; ASTM D624
 258 pliDie B, post cured- 4 hours at 177°C; ASTM D624
Compression Set 60 %no post cure; ASTM D395
 
Thermal PropertiesOriginal ValueComments
Shrinkage 1.7 %no post cure
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMULTI169 / 54073

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.