MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chevron Phillips Marlex® 1010 LDPE Extrusion Coating Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Resin Type: High Speed Resin

Characteristics: Excellent Processability, High Temperature Extrusion Stability, Good Draw Down Resin

Applications: Food Packaging, Laminations

Data provided by Chevron Chemical.

Formerly branded with the MarFlex® trade name.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D1505-60T
Melt Flow 10 g/10 min10 g/10 minASTM D1238-57T
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 9.30 MPa1350 psiASTM D638-61T
Tensile Strength, Yield 7.60 MPa1100 psiASTM D638-61T
Elongation at Break 650 %650 %ASTM D638-61T
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 128 °C262 °FASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Carmel Olefins Ipethene® 213 Low Density Polyethylene
Carmel Olefins Ipethene® 210 Low Density Polyethylene
Carmel Olefins Ipethene® 113 Low Density Polyethylene
Carmel Olefins Ipethene® 111 Low Density Polyethylene
Carmel Olefins Ipethene® 100 Low Density Polyethylene

PCHEVVE2 / 20537

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.