MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik ALBIFLEX® 296 DGEBA Epoxy-Silicone Block Copolymer
Categories: Polymer; Thermoset; Epoxy; Silicone

Material Notes: Most ALBIFLEX® products are epoxy-silicone block copolymers that can be used to formulate high performance elastomers. They can be cured with most commercially available epoxy hardeners, except aromatic amines. Systems with an outstanding combination of properties can be designed:
  • high thermal shock resistance and temperature stability
  • hardness between Shore A 70 and D 60, depending on the curing agent used, with excellent elongation
  • high mechanical stability
  • excellent adhesion on most substrates
  • lower water vapor permeability than that of silicones
  • very low moisture absorption
Upon curing, ALBIFLEX® 246, 296, and 348 form a segmented molecular structure consisting of soft polysiloxane and rigid polyepoxy segments. When the polysiloxane and epoxy units in the polymer structure are combined, an elastomeric material is created that has both the outstanding electrical and thermal properties of silicones and the high mechanical strength and excellent adhesion of epoxy resins.

Application: ALBIFLEX® products are used in all applications where improved flexibility or toughness of the cured resin is desired without sacrificing other properties and to formulate unique adhesives and sealants. Examples of possible uses for ALBIFLEX® include:

  • fibre-reinforced materials and composites
  • applications in electrical/electronic equipment, for example, casting, potting, encapsulation
  • structural adhesives

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 45000 cP
 
Descriptive Properties
Content100%Si/EP-copolymer content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIL626 / 196830

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.