MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling Trovidur® EA PVC
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Product characteristics:
  • High UV and weather resistance
  • Good glueability
  • Fire class B1 according to DIN 4102 up to 4 mm thickness
Product applications:
  • Construction industry

Information provided by Röchling.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.47 g/ccDIN EN ISO 1183-1
Water Absorption <= 0.20 %DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.0 MPaDIN EN ISO 527
Elongation at Break 15 %DIN EN ISO 527
Modulus of Elasticity 3.20 GPaDIN EN ISO 527
Izod Impact, Notched (ISO) 4.00 kJ/m²DIN EN ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmDIN EN 62631-3-1
Surface Resistance >= 1.00e+13 ohmDIN EN 62631-3-2
Dielectric Constant 3.2IEC 60250
Dissipation Factor 0.020
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 80.0 µm/m-°CDIN 53752
Thermal Conductivity 0.160 W/m-KDIN 52612-1
Maximum Service Temperature, Air 60.0 °Clong term
Vicat Softening Point 80.0 °CDIN EN ISO 306, Vicat B
Minimum Service Temperature, Air -15.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PVC, Wire and Cable Grade
Röchling Trovidur® ET PVC
Röchling Astrawood® PVC-U
Overview of materials for Cyclo Olefin Polymer
Omnia Plastica PVC Polyvinylchloride

PROCH9352 / 233054

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.