MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Thermal Ceramics Cera-Kote 332-D
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Cera-Kote 322-D is a white, high viscosity, high strength premium grade cement.

Features:

  • Range of grades with different viscosities
  • Develops strong bond on drying
  • Long shelf life when properly stored
  • Applications:

  • Adhesive to apply foils (stainless or aluminum) to Kaowool ceramic fiber blanket
  • Adhesive to join vacuum formed Kaowool ceramic fiber parts together
  • Adhesive and insulation for heating elements
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Mechanical PropertiesOriginal ValueComments
    Modulus of Rupture 0.255 ksiBond strength, after air drying
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 3250 °F
    Maximum Service Temperature, Air 2200 °F
    Shrinkage 2.5 %
    @Temperature 1260 °C,
    Time 86400 sec
     
    Processing PropertiesOriginal ValueComments
    Drying Temperature 150 °F
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 44 %
    Other 2.0 %
    SiO2 55 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    CTHERM263 / 2583

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.