MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Excelite Plastic Polycarbonate Light Diffusion sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Excelite light diffusion PC sheet is contains many tiny diffuser beads that continually change the light propagation. That ensures optimum light diffusion. It turns light into a unique experience. Soft, pleasant lighting devoid of harsh shadows makes for agreeable surroundings. Different light sources complement each other harmoniously. What is more, thanks to its high light transmission and excellent light diffusion, it is significantly cuts energy costs when employed as a luminaries cover or illuminated sign. PC diffusion sheet is the most durable sheet in advertising application in the market. It can relieve spot lighting belt and reduce light pollution to make the light soft and diffuse. It is the best material for the LED light box for advertisement.

Features:

  • High light transmission
  • High Impact Resistance, practically unbreakable
  • Restful to the eye, mood-enhancing
  • Long service life time
  • Large range of sheet sizes & thicknesses
  • 10 Year Warranty
  • Light weight
Applications
  • LED Advertising light box
  • Privacy Glazing
  • Luminaries
  • Illuminated signage
  • Light Diffuser in architectural light fittings
  • Spotlights
  • Lamp chimney

Information provided by Excelite Plastic Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccGB/T 1033
Water Absorption 0.30 %
@Time 86400 sec
GB/T 1033
Thickness 1500 - 12000 microns
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 60.3 MPaGB/T 1040
Elongation at Break >= 90 %GB/T 1040
 108 %Tensile; GB/T 1040
Elongation at Yield 6.0 %GB/T 1040
Modulus of Elasticity 0.240 GPaGB/T 9341
 
Thermal PropertiesOriginal ValueComments
CTE, linear 63.0 µm/m-°CGB/T 1034
 
Descriptive Properties
ColorOpal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teijin Panlite® ML-1105 Light Diffusion Grade Polycarbonate
Teijin Panlite® ML-1103 Light Diffusion Grade Polycarbonate
Teijin Panlite® ML-1102 Light Diffusion Grade Polycarbonate
Teijin Panlite® LN-3000RM High Light Reflection, Halogen-Free Flame Resistant Polycarbonate Resin
Teijin Panlite® LN-1010RM High Light Reflection, Flame Resistant Polycarbonate Resin

PEXLT007 / 198717

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.