MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem AKROCHEM® DDPH-50 Cross-linking agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Akrochem DDPH is a liquid dialkyl peroxide, 2,5-dimethyl-2,5-di(tert-butylperoxy) hexane, for use as a cross-linking agent for synthetic and natural rubbers. Akrochem DDPH-50 is a dispersion of the liquid peroxide on calcium carbonate. The dispersed form provides improved handling characteristics and properties associated with powdered compounding ingredients. [Note: The true active peroxide is 45- 46% in the DDPH-50 product. This is because the pure liquid is approx. 92% active. The pure product is always cut for safer handling].

Applications: Akrochem DDPH peroxide is used as a catalyst for cross-linking a variety of synthetic rubbers including EPR, EPDM, EVA, NBR, polychloroprene, PVC, chlorosulphonated polyethylene, SBR, polyurethane, and silicone. The powdered form provides ease of handling and weighing accuracy. DDPH peroxide is a low odor catalyst and due to its aliphatic structure, imparts a minimal amount of discoloration in the final cure. Typical dosages range from 1.0 to 10.0 phr depending on polymer type and filler loadings. In its liquid form, DDPH is a clear, colorless liquid which can be used as a cure catalyst in applications where optical clarity is essential. Unlike Bis (t-butylperoxy) diisopropylbenzene peroxide (“Vulcup” type), DDPH peroxide will not bloom from EPDM's. In silicones, only vinyl-containing polymers can be cured. In peroxide-curable FKM, use 2.5 phr DDPH-50 peroxide along with 4 phr coagent Akrosorb 19251 (72% TAIC). DDPH is acceptable under FDA 177.2600 Regulations, Sec.(b) "Accelerators" under the chemical name: (1,1,4,4-Tetramethyltetramethylene) bis-tert-butyl peroxide.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.50 g/cc
 
Descriptive Properties
Appearancepowder
Carrier Typecalcium carbonate
Content0.45Peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH562 / 315480

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.