MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chesterton ARC 897 Fine Grade Sliding Wear Compound  (discontinued **)
Categories: Ceramic; Polymer; Thermoset; Epoxy

Material Notes: Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a thickness of 3 mm (1/8”) or more. Non-shrinking. 100% Solids. ARC 897 is formulated with a high concentration of small ceramic beads and particles for extremely abrasive environments where metal loss is often repaired by more conventional and costly weld overlay. ARC 897 can be used either to rebuild eroded metal surfaces or to provide a wear resistant, sacrificial surface which frequently outperforms the original metal, rubber liners, ceramic tiles or weld overlay. ARC 897 is a long lasting wearing surface and is chosen over ARC 890 where a thinner, more easily applied composite is required.

Benefits:

  • Excellent wear characteristics of ARC 897 extends equipment operating cycles.
  • Tough resin structures resists thermal-mechanical shock
  • Outstanding adhesion results in reliable performance with no undercutting
  • Ease of application reduces labor and downtime costs
  • It can be easily shaped and formed to any metal surface.

Suggested Uses:

  • Pneumatic Conveyors
  • Chipper and Chip Bins
  • Hydro Pulpers
  • Turbo Separators
  • Ni-Hard Slurry Pumps
  • Fly Ash Separators
  • Wood Chip Transport Fans
  • Screws Conveyors
  • Exhaust Fans
  • Cyclones, Hoppers
  • Wear Plates
  • Pipe Elbows
  • Pulverized Fuel Lines
  • Pulverizers

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Hardness, Shore D 9090ASTM D2240
Tensile Strength at Break 33.1 MPa4800 psiASTM D638
Flexural Strength 67.6 MPa9800 psiASTM D790
Compressive Strength 93.1 MPa13500 psiASTM D695
Impact Test 5.99 J4.42 ft-lbReverse; ASTM D2794
 
Thermal PropertiesMetricEnglishComments
CTE, linear 39.6 µm/m-°C22.0 µin/in-°FASTM C531
Maximum Service Temperature, Air 95.0 °C203 °FWet Service
 205 °C401 °FDry Service
 
Processing PropertiesMetricEnglishComments
Cure Time  90.0 min
@Temperature 43.0 °C
1.50 hour
@Temperature 109 °F
Light Load
 360 min
@Temperature 32.0 °C
6.00 hour
@Temperature 89.6 °F
Light Load
 480 min
@Temperature 25.0 °C
8.00 hour
@Temperature 77.0 °F
Light Load
 720 min
@Temperature 43.0 °C
12.0 hour
@Temperature 109 °F
Full Load
 1200 min
@Temperature 32.0 °C
20.0 hour
@Temperature 89.6 °F
Full Load
 1440 min
@Temperature 16.0 °C
24.0 hour
@Temperature 60.8 °F
Light Load
 1440 min
@Temperature 43.0 °C
24.0 hour
@Temperature 109 °F
Full Chemical
 1800 min
@Temperature 32.0 °C
30.0 hour
@Temperature 89.6 °F
Full Chemical
 2160 min
@Temperature 10.0 °C
36.0 hour
@Temperature 50.0 °F
Light Load
 2160 min
@Temperature 25.0 °C
36.0 hour
@Temperature 77.0 °F
Full Load
 2880 min
@Temperature 16.0 °C
48.0 hour
@Temperature 60.8 °F
Full Load
 2880 min
@Temperature 25.0 °C
48.0 hour
@Temperature 77.0 °F
Full Chemical
 4320 min
@Temperature 10.0 °C
72.0 hour
@Temperature 50.0 °F
Full Load
 4320 min
@Temperature 16.0 °C
72.0 hour
@Temperature 60.8 °F
Full Chemical
 5760 min
@Temperature 10.0 °C
96.0 hour
@Temperature 50.0 °F
Full Chemical
Tack-Free Time  19.8 min
@Temperature 43.0 °C
0.330 hour
@Temperature 109 °F
 120 min
@Temperature 32.0 °C
2.00 hour
@Temperature 89.6 °F
 240 min
@Temperature 25.0 °C
4.00 hour
@Temperature 77.0 °F
 420 min
@Temperature 16.0 °C
7.00 hour
@Temperature 60.8 °F
 960 min
@Temperature 10.0 °C
16.0 hour
@Temperature 50.0 °F
 
Descriptive Properties
ColorGray

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS024 / 138136

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.