System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Multibase Multi-Flex® TPO D 5305
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Thermoplastic Olefinic Elastomer (TPO)
Material Notes:
Multi-Flex® D 5303 is a TOP compound for automotive applications such as bumper covers and side panels.
Data provided by Multibase.
Key Words:
Thermoplastic Polyolefin
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.06
g/cc
0.0383
lb/in³
ASTM D792-91
Melt Flow
5.0
g/10 min
5.0
g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
54
54
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate
17.9
MPa
2600
psi
20" / min.; ASTM D-683-95
Elongation at Break
260 %
260 %
ASTM D638-95
Flexural Modulus
1.021
GPa
148.1
ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched
NB
NB
ASTM D-256-93a
Gardner Impact
20.9
J
15.4
ft-lb
ASTM D5420
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Multibase Multi-Flex® TPE D 6606 BLK
Multibase Multi-Flex® TPE D 6208 BLK
Borealis Daplen™ EE040AE TPO Compound
PLA222 / 49619
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.