MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chemours Teflon™ PFA C-980 Perfluoroalkoxy fluoropolymer resins
Categories: Polymer; Thermoplastic; Fluoropolymer; Perfluoroalkoxy (PFA); Polyperfluoroalkoxyethylene, Molded/Extruded

Material Notes: Teflon™ PFA C-980 (perfluoroalkoxy) fluoropolymer resins combine the chemical and high temperature resistance of Teflon™ PFA with anti-static levels of electrical conductivity. Anti-static linings of components used in the chemical processing industries; industrial film; articles requiring superior electrical, chemical, and thermal properties.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.15 g/ccASTM D792
Water Absorption <= 0.030 %
@Time 86400 sec
ASTM D570
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 372 °C
ASTM D3307
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ASTM D2240
Tensile Strength 36.0 MPaASTM D3307
Elongation at Break 300 %ASTM D3307
Flexural Modulus 0.586 GPaASTM D790
Flex Crack Resistance 80000Cycles MIT Folding Endurance; ASTM D2176
Izod Impact, Notched NBASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square >= 1.00e+17 ohmASTM D257
Dielectric Constant 2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 80.0 kV/mm
@Thickness 0.100 mm
ASTM D149
Dissipation Factor 0.00010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Melting Point 284 °CASTM D4591
Flammability, UL94 V-0
Oxygen Index >= 95 %ASTM D240
 
Descriptive Properties
Chemical/Solvent ResistanceExcellentASTM D543
Critical Shear Rate (1/s)12372°C
Heat of Combustion5.3 MJ/kgASTM D240
Salt Spray Resistance Coatings (hours)1000ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather and Chemical ResistanceExcellent
Weather Resistance (years unaffected)10Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDU8812 / 268738

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.