MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Magnesium AM100A-T61, Sand Cast
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: AM100A-T61 is pressure tight, with a good combination of strength and elongation. Can be cast as permanent-mold (AMS 4483, ASTM B 199), investment cast (AMS T6 temper, 4455, ASTM B 403), Sand cast (ASTM B 80). No longer widely used, typical uses were commercial and military pressure-tight sand and permanent mold structural castings with good combinations of tensile strength, yield strength, and elongation. Very good weldability.

Key Words: UNS M10100; SAE J465; Mg; Old SAE 502; AMS 4483; ASTM B 80; ASTM B 199; AMS 4455 T6 temper; ASTM B 403 (Ingot UNS M10101)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.83 g/cc0.0661 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 6969500 kg load, 10 mm ball
Hardness, Knoop 9292Estimated from Brinell
Hardness, Rockwell E 8080
Hardness, Vickers 7979Estimated from Brinell
Tensile Strength, Ultimate 275 MPa39900 psi
Tensile Strength, Yield 150 MPa
@Strain 0.2 %
21800 psi
@Strain 0.2 %
Elongation at Break 1.0 %1.0 %in 50 mm
Tensile Modulus 45.0 GPa6530 ksi
Compressive Yield Strength 150 MPa21800 psiat 0.2% offset
Ultimate Bearing Strength 560 MPa81200 psi
Bearing Yield Strength 470 MPa68200 psi
Poissons Ratio 0.350.35
Fatigue Strength 70.0 MPa
@# of Cycles 5.00e+8
10200 psi
@# of Cycles 5.00e+8
R.R. Moore Test
Machinability 100 %100 %Relative Rating, 100=Best
Shear Modulus 17.0 GPa2470 ksi
Shear Strength 145 MPa21000 psi
Charpy Impact 0.900 J0.664 ft-lbV-notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000150 ohm-cm0.0000150 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 372 J/g160 BTU/lb
CTE, linear  25.0 µm/m-°C
@Temperature 0.000 - 100 °C
13.9 µin/in-°F
@Temperature 32.0 - 212 °F
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
15.0 µin/in-°F
@Temperature 68.0 - 392 °F
Estimated from similar Mg alloys
Specific Heat Capacity 1.05 J/g-°C0.251 BTU/lb-°F
Thermal Conductivity 73.0 W/m-K507 BTU-in/hr-ft²-°F
Melting Point >= 430 °C>= 806 °FIncipient Melting
Solidus 463 °C865 °F
Liquidus 595 °C1100 °F
 
Processing PropertiesMetricEnglishComments
Casting Temperature 735 - 845 °C1360 - 1550 °FSand Casting
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 9.3 - 10.7 %9.3 - 10.7 %
Copper, Cu <= 0.10 %<= 0.10 %
Magnesium, Mg 90 %90 %As Remainder
Manganese, Mn >= 0.10 %>= 0.10 %
Nickel, Ni <= 0.010 %<= 0.010 %
Silicon, Si <= 0.30 %<= 0.30 %
Zinc, Zn <= 0.30 %<= 0.30 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium AM100A-T4, Cast
Magnesium AM100A-F, Cast
Magnesium AS41XA-F, Die Cast
Magnesium AM100A-T6, Cast
Magnesium AM100A-T7, Cast

MMAM10 / 12291

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.