Halogen-free, flame retardant, radiation cross-linkable compound Compound class: Insulation / sheathing Compound category: RDX Flame retardant: ATH Standards: IEC 60092/360 Table II, SHF2 UL 1277 Typical applications: The compound can be an ideal solution for applications like coax cables, electronic cables, communication cables, low voltage power cables, instrumentation and control cables in harsh environments. Features: Flame retardant; Halogen-free; Low smoke; Oil resistant; High temperature resistant Information provided by Melos |