MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Silfar® SE 4 Simeticone Emulsion
Categories: Fluid

Material Notes: SILFAR® SE 4 is a silicone antifoam emulsion. It is recommended for the food and pharmaceutical sectors, fermentation processes and agrochemical formulations.

Properties: SILFAR® SE 4 complies with the requirements set down in the monographs "Simethicone Emulsion" (USP) and its components comply with EP. SILFAR® SE 4 conforms to FDA 21 CFR § 173.340 "Defoaming Agents" as a "Secondary Direct Food Additive Permitted in Food for Human Consumption." SILFAR® SE 4 only contains substances listed in the Directive 95/2/EC and Amendments. SILFAR® SE 4 complies with the Recommendations of the BfR concerning the manufacture of essential commodities that have contact with food as follows: XV. Silicones. SILFAR® SE 4 meets the criteria for an exemption from the requirements of a tolerance when used as an additive in pesticide formulations to be applied to growing crops or raw agricultural commodities after harvest as specified in 40 CFR 180.910. National regulations applicable in the countries concerned must be observed.

Application: SILFAR® SE 4, a simethicone emulsion is used in antiflatulence and antacid preparations. It works by acting as an antifoam agent to prevent or relieve flatulence in alimentary canal and by forming a protective lining on e.g. the gastric mucous membrane. It is often combined with fermentation preparations. When administered to patients, preparations containing the antifoam SILFAR® SE 4 eliminate any flatulence that might hinder X-ray, ultrasonic or gastroscopic examinations. SILFAR® SE 4 may also be used to make liquid preparations in suspension form. It serves in veterinary medicine to prevent bloat in cattle and sheep and may be added to the water in the trough. SILFAR® SE 4 is also an antifoam in fermentation and downstream processes, such as active-ingredient extraction and solvent recovery, especially when USP/EP compliant products are mandatory. SILFAR® SE 4 is used in strongly foaming, aqueous systems in the food

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³DIN 57175
Solids Content 31 - 34 %31 - 34 %
pH 3.0 - 5.03.0 - 5.0
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Active ingredients (%)30
Appearancemilky white, light yellowish
Content<100 CFU/gMicrobe count

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9436 / 204965

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.