MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Goodfellow Manganin® Copper Resistance Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Copper Alloy

Material Notes: Resistance alloy with moderate resistivity and low temperature coefficient. The resistance/temperature curve is not as flat as the constantans nor are the corrosion resistance properties as good.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.40 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 300 - 600 MPa
Elongation at Break <= 50 %
Tensile Modulus 124 - 159 GPa
Izod Impact, Unnotched 1.07 J/cmNotch Status Unknown
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000430 - 0.0000480 ohm-cmTemperature Coefficient of 0.00001/K
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 - 19.0 µm/m-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 22.0 W/m-K
Melting Point 960 °C
Maximum Service Temperature, Air 300 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 86 %
Manganese, Mn 12 %
Nickel, Ni 2.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Constantan Thermocouple Wire
Goodfellow T1-Thermocouple Alloy
California Fine Wire Manganin 290 Copper, Manganese, and Nickel Resistance Wire
Sandvik Manganin® 43 Resistance Wire
202 Stainless Steel, Annealed Bar

NGOODF174 / 16244

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.