MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker ELASTOSIL® R 865/50 HCR Silicone
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® R 865/50 offers numerous functional advantages. The material ensures superior rebound resiliency and a minimal compression set. The compounds are easily pigmentable with ELASTOSIL® PT Pigment Pastes and have good processing characteristics. The various grades (ELASTOSIL® R 865/40 - ELASTOSIL® R 865/70) can be blended in any proportion to achieve intermediate hardnesses.

Application: ELASTOSIL® R 865/50 is especially designed for peroxide curing applications as

  • calendaring
  • molding

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccDIN 51757
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050DIN 53505
Tensile Strength 8.20 MPa1190 psiDIN 53404 S1
Elongation at Break 390 %390 %DIN 53404 S1
Rebound 65 %65 %DIN 53512
Tear Strength 17.0 kN/m97.0 pliASTM D624 B
Compression Set 12 %
@Temperature 175 °C,
Time 79200 sec
12 %
@Temperature 347 °F,
Time 22.0 hour
DIN ISO 815-B
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 165 °C
0.250 hour
@Temperature 329 °F
0.5% ELASTOSIL® AUX Crosslinker C6; Post-Cured 4h/200 ºC
 
Descriptive Properties
AppearanceTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9917 / 197516

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.