Moplen RP3231 is a polypropylene random copolymer used for extrusion applications. Moplen RP3231 has a very narrow molecular weight distribution and is formulated with an anti-gas fading stabilization package. Moplen RP3231 is used for the production of soft textile filaments. Typical application is spun bonded nonwovens. Applications: Filament Yarn, Hygiene Nonwoven, Nonwovens.Information provided by LyondellBasell. |