MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CHT HANSA CARE 3010 Organo modified Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: Organo modified Silicone for the use as ingredient in Home and Car Care products. The silicone chemistry allow to formulate high end products with unique effects.

Key Features

  • Emulsifier for W/O emulsions
  • Improves Polishing
  • Emulsion stabilizer
  • Enhances Gloss
Key Applications
  • Car Polishes
  • Leather and Furniture Care
  • Vinyl and Tyre Care
Application: HANSA CARE 3010 is an ideal emulsifier for W/O emulsions. It is ideal to emulsify aliphatic solvents. Emulsions made with HANSA CARE 3010 show very good stability and an easy polishing. HANSA CARE 3010 can be used in cold or hot processes.

Addition Rates:
Dosage – 1: 1.0 - 5.0% as emulsifier

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles 10 %10 %
Brookfield Viscosity <= 2000 cP<= 2000 cP
Storage Temperature 4.00 - 40.0 °C39.2 - 104 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceColorless to yellow liquid
ChemistryAlkyl and polyether modified siloxane
IonicityNon-ionic
MIT FreeYes
Ultralow cyclic contentNo

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL372 / 314855

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.