MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultramid® STAR AF 219 V30 NATURAL Nylon 66, 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Product Description: Ultramid® STAR AF 219 V30 NATURAL is based on a high flow polyamide 6.6 resin, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This grade has enhanced molding behaviors and better surface aspect. It offers an excellent combination between thermal and mechanical properties. This grade restricts electrolytic corrosion.

Availability: Africa & Middle East; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber, 30% Filler by Weight

Features: Electrical Corrosion Resistant; Heat Stabilized – Organic; High Flow; Outstanding Surface Finish

Uses: Automotive Applications; Connectors; Electrical/Electronic Applications; General Purpose; Pulleys

Agency Ratings: EC 1907/2006 (REACH); EU 2011/65/EC; EU 2015/863 RoHS3

RoSH Compliance: RoSH Compliant

Appearance: Natural Color; Black

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66-GF30

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccISO 1183
Water Absorption 1.9 %Equilibrium, 50% RH; ISO 62
 0.80 %
@Time 86400 sec
ISO 62
Maximum Moisture Content 0.20
Linear Mold Shrinkage, Flow 0.0095 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0028 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 26800 psiISO 527-2
Elongation at Break 2.6 %ISO 527-2
Tensile Modulus 1.45e+6 psiISO 527-1
Flexural Strength 39200 psiISO 178
Flexural Modulus 1.31e+6 psiISO 178
Izod Impact, Unnotched (ISO) 24.0 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 29.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 3.80 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VSolution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 496 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 482 °FUnannealed; ISO 75-2/A
 486 °FUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 509 - 527 °F
Middle Barrel Temperature 518 - 536 °F
Front Barrel Temperature 536 - 554 °F
Mold Temperature 140 - 194 °F
Drying Temperature 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2050 / 310743

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.